富美家防火板的耐热、耐磨、耐刮、耐感染、抗冲击、防水等各项性能相对与其他的表面装饰材料有突出的优势,所以在市场中的购买前景不错,下面就来讲讲生产防火板时候容易出现三个问题,做好预防措施。
The heat resistance, abrasion resistance, scratch resistance, infection resistance, impact resistance, water resistance and other properties of Fumeijia fire-proof board have outstanding advantages compared with other surface decoration materials, so the purchase prospect in the market is good. Now let's talk about three problems that are easy to occur in the production of fire-proof board, and take preventive measures.
一、板面局部有白花
1、 There are some white flowers on the board surface
产生的原因:
Causes:
1、表层纸含胶量不足或干燥中局部树脂固化
1. Insufficient glue content of surface paper or partial resin curing during drying
2、表层纸挥发物含量过低
2. The volatile content of surface paper is too low
3、热压式压力不均匀
3. Uneven hot pressing pressure
4、忖垫材料无弹性
4. The cushion material is inelastic
5、不锈钢板表明不平
5. Stainless steel plate indicates unevenness
6、树脂反应过老,分子太大,树脂流动性大
6. The resin reaction is too old, the molecule is too large, and the resin fluidity is large
解决的方法:
Solution:
1、提高表层纸树脂含量或控制干燥温度,防止局部树脂固化
1. Increase resin content of surface paper or control drying temperature to prevent local resin solidification
2、提高表层纸的挥发物含量
2. Improve the volatile content of surface paper
3、检修热压机,改进加压面的均匀性
3. Overhaul the hot press and improve the uniformity of the pressure surface
4、定期更换忖垫材料
4. Replace the cushion material regularly
5、不锈钢板定期抛光
5. Regular polishing of stainless steel plate
6、树脂应分析检验,不合格指标要求时停止使用
6. The resin shall be analyzed and inspected, and it shall not be used when it is unqualified
在生产防火板的过程中易出现的问题
Problems easy to occur in the production of fireproof boards
二、板面有湿花(水汽),边缘较为严重
2、 There are wet streaks (moisture) on the board surface, and the edges are relatively serious
产生的原因:
Causes:
1、浸胶纸干燥后挥发物含量太高
1. The volatile content of the impregnated paper is too high after drying
2、印刷木纹的油墨或染料所用的溶剂不合适
2. The solvent used for printing wood grain ink or dye is inappropriate
3、浸胶干燥后的胶膜纸吸湿(回潮)
3. Moisture absorption (moisture regain) of impregnated and dried adhesive film paper
解决的方法:
Solution:
1、降低浸胶纸干燥后的挥发物含量
1. Reducing Volatile Content of Dried Impregnated Paper
2、调换油墨(染料)用的溶剂
2. Solvent for changing ink (dye)
3、注意胶膜纸的存放,一般可用塑料布遮盖
3. Pay attention to the storage of adhesive film paper, which can generally be covered with plastic cloth
在生产防火板的过程中易出现的问题
Problems easy to occur in the production of fireproof boards
三、装饰板表面开裂
3、 The surface of the decorative plate is cracked
产生的原因:
Causes:
1、树脂反应过嫩,分子太小
1. The resin is too tender and the molecule is too small
2、树脂固化不完全
2. Incomplete resin curing
3、表层胶膜纸含胶量太高
3. The adhesive content of the surface adhesive film paper is too high
解决的方法:
Solution:
1、不合格的树脂停止使用
1. Unqualified resin shall not be used
2、适当提高热压温度或延长热压时间
2. Properly increase the hot pressing temperature or extend the hot pressing time
3、控制表层胶膜纸的含胶量
3. Control the glue content of the surface adhesive film paper
生产防火板时候容易出现三个问题就是以上所讲解的内容了,您对此有什么想咨询的地方或者有采购需求,都可以来我们网站https://www.fumeijia.net看看。
There are three problems that are easy to occur in the production of fireproof boards. If you have any questions or purchase needs, you can come to our website https://www.fumeijia.net have a look.