1.开料时,应以直线锯切为主。通常可先在这种板材上画好规格尺寸,然后再锯切,如果工件的尺寸为标准尺寸,可先用模板划线,再进行锯切,这会方便得多。
1. During cutting, straight sawing shall be the main method. Generally, you can draw the specifications and dimensions on this kind of plate before sawing. If the size of the workpiece is standard, you can draw a line with the template before sawing, which is much more convenient.
2.开孔时,可利用手提曲线锯进行切割,切割速度以3-4m/min为宜,如切割速度过快,一方面会使切割边缘产生爆口等缺陷,另一方面也会影响锯条的使用寿命,增加加工成本。
2. When opening holes, the portable curve saw can be used for cutting, and the cutting speed should be 3-4 m/min. If the cutting speed is too fast, on the one hand, it will cause defects such as bursting at the cutting edge, on the other hand, it will also affect the service life of the saw blade and increase the processing cost.
3.加工异形边沿时,应先在板件表面划出所需尺寸,然后利用曲线锯切割;如果批量生产时,可利用模板进行切割,这样可确保加工速度和锯切质量。
3. When processing the irregular edge, the required size should be marked on the surface of the plate first, and then cut with a curve saw; In case of mass production, the template can be used for cutting, which can ensure the processing speed and sawing quality.
4.加工边缘时,普遍采用的工具是手提镂铣机,在作业前,应清除板件表面的灰尘或异物。以免在抗倍特板件表面留下划痕或刻痕,镂铣机的加工速度应保持在2m/min为宜,如果镂铣刀刀刃角度较小而工件厚度又较厚时,镂铣机的加工速度应适当放慢。另外,铣刀刃的长度应大于加工件的厚度,以保证一次走刀能铣削出边缘的线型。走刀时,镂铣刀应从高处逐步向低处下滑直至镂铣刀刃包容铣削边缘。值得注意的是,走刀时,一定要保持平稳,不要让镂铣机晃动,晃动会使工件的边缘形成不规则波纹,给后道砂磨抛光工序增加工作量,影响加工效率。
4. When processing edges, the commonly used tool is a portable router. Before operation, dust or foreign matters on the surface of the plate should be removed. In order to avoid leaving scratches or nicks on the surface of the anti-magnification plate, the processing speed of the router should be kept at 2 m/min. If the cutting edge angle of the router is small and the workpiece thickness is thick, the processing speed of the router should be appropriately slowed down. In addition, the length of the milling cutter edge should be greater than the thickness of the workpiece to ensure that the edge line can be milled at one time. When cutting, the router shall slide down from high to low gradually until the router edge covers the milling edge. It is worth noting that when cutting, it must be kept stable. Do not let the router shake. The shaking will cause irregular ripples on the edge of the workpiece, which will increase the workload of the subsequent sanding and polishing process and affect the processing efficiency.
以上就是相关的在处理抗倍特板时应注意的一些问题解答了,希望给您帮助,更多相关事项就来我们网站https://www.fumeijia.net咨询吧!